We supply lron Oxides for Soft Ferrites of which specification is as shown below..

 

 

Chemical Composition

          Grade

       DOALOX - 100

     DOALOX - 80

          Fe2O3

        99.2 min.

       99.2 min.

          SiO2

   100 ppm max.

      80 ppm max.

         Al2O3

        40 ppm max.

      40 ppm max.

         CaO

      100 ppm max.    

      70 ppm max.  

         MnO

    2,500 ppm max.

   2,500 ppm max.

         Na2O

  100 ppm max.

       70 ppm max.

        Cl

        0.10 % max.

        0.10 % max.

 

 

Physical Properties

Moisture Content

          0.4 % max.

          0.4 % max.

  Average Particl Size

          0.6~1.0m

          0.6~1.0m

    Surface Area

       3.5~4.5 m2/g

       3.5~4.5 m2/g

  Averge Bulk Density

          0.45 g/cm3

         0.45 g/cm3

 

      Our iron oxides are produced by Roaster type Hydrochloric Acid Regeneration Plant with
      Silica Reduction System in a steel cold rolling mill and we assure you that we can guarantee